REFRACTORY GRADECHROME OXIDE GREEN

DELIKEOXIDE® — 9 GRADES · 2 Cr(VI) TIERS

Sintered Cr₂O₃ for the hottest linings on Earth. Nine particle-size windows across two Cr(VI) tiers, engineered for chrome-magnesia bricks, castables, ramming mixes and kiln furniture in continuous service above 1700 °C.

Refractory grade chrome oxide green — sintered Cr₂O₃ grit production
Fig. 01 — Sintered Cr₂O₃ grit before screening · DELIKEOXIDE refractory line

WHY Cr₂O₃IN REFRACTORIES

In a refractory lining, chrome oxide green is not a colour — it is a structural oxide. Cr₂O₃ melts at 2435 °C, grades 8.5–9 on Mohs, and stays chemically inert against the most aggressive ferrous slags in steelmaking.

01

2435 °C MELTING

The oxide does not soften anywhere near lining service — Cr₂O₃ keeps its identity in systems running continuously above 1700 °C.

02

MOHs 8.5–9

Hardness at the level of corundum: chrome oxide grit builds dense, erosion-resistant hot faces, not crushable aggregate.

03

SLAG INERTNESS

Low solubility in FeO-rich and fayalite melts, plus a self-sealing spinel skin — the mechanism is explained below.

04

≤5 ppm Cr(VI) OPTION

Low-Cr(VI) grades keep hexavalent chromium at ≤5 ppm for plants enforcing strict occupational-exposure and waste rules.

VerdeChrome supplies nine DELIKEOXIDE refractory chrome oxide green grades in two Cr(VI) tiers. The standard tier (G-5001, G-5002, G-5003, G-5006) holds Cr₂O₃ ≥99 % with Cr(VI) ≤200 ppm; the Low-Cr(VI) tier (G-5891, G-5899, G-5996, G-5070, G-5073) caps hexavalent chromium at ≤5 ppm. Both tiers are sintered to closed porosity, so the grit performs as dense aggregate — not pigment powder. Grade selection is a particle-size decision: coarse windows build the skeleton of ramming mixes, mid windows fill brick matrices, sub-micron powders pack the voids. The table below maps each window to its forming method.

NINE GRADESTWO TIERS

Nine particle-size windows, two Cr(VI) ceilings. All grades are sintered Cr₂O₃, screened and laser-checked per lot. Download the TDS for any grade.

GRADETIERD50Cr(VI)Cr₂O₃TYPICAL USETDS
G-5001Standard1.2 μm≤200 ppm≥99 %Fine fraction for dense matrix packing in bricks and castables
G-5002Standard2–3 μm≤200 ppm≥99 %General matrix component; balanced fines for pressed brick bodies
G-5003Standard3–4 μm≤200 ppm≥99 %Castable matrix; intermediate grit between coarse and fine fractions
G-5006Standard4–8 μm≤200 ppm≥99 %Coarse grit: ramming mixes, taphole bodies, kiln furniture
G-5891Low-Cr(VI)1–2 μm≤5 ppm≥99 %Fine filler where occupational-exposure limits are strict
G-5899Low-Cr(VI)3–8 μm≤5 ppm≥99 %Coarse fraction for ramming mixes under strict waste rules
G-5996Low-Cr(VI)3–4 μm≤5 ppm≥99 %Low-Cr(VI) castable matrix; drop-in for G-5003
G-5070Low-Cr(VI)0.1–3 μm≤5 ppm≥98.5 %Micropowder for maximum packing density and low porosity
G-5073Low-Cr(VI)0.1–0.6 μm≤5 ppm≥98.5 %Sub-micron reactive fines; dense coatings on kiln furniture
Custom gradation

Need a distribution that is not in the table? We blend and screen to your sieve curve and match your target PSD within one production cycle. Full series context on the refractory series page.

CHROME-MAGNESIAAPPLICATIONS

Chrome-magnesia refractories pair periclase with chrome oxide to exploit a simple fact: MgO resists basic slag, Cr₂O₃ resists iron-rich slag — together they resist both.

STEELRH Degassers+30–50 % campaign lifeDirect-bonded chrome-magnesia bricks in snorkels and lower vessels — linings with VerdeChrome Cr₂O₃ hold 30–50 % longer campaigns than periclase-spinel.Read the RH degasser field notes.
STEELAOD / VOD Vessels>1700 °C serviceConverter linings that see molten metal, FeO-rich slag and thermal cycling in the same campaign — the standard case for chrome oxide in the matrix.See the refractory engineering guide.
NONFERROUSCu / Ni ConvertersTuyere zonesCopper and nickel converter tuyere zones: chrome oxide tolerates the fayalite-rich slag that strips plain magnesia.Grades: G-5003 / G-5996 matrix, G-5001 fines.
CEMENTRotary Kiln Burning ZoneClinker coating stabilityChrome oxide stabilises the protective clinker coating in the burning zone against alkali sulphates and liquid clinker phases.See burning zone analysis.
MONOLITHICSCastables & Ramming MixesBimodal packingCoarse G-5006 / G-5899 grit for the skeleton, G-5001 or G-5070 fines to pack the voids: denser, stronger, tighter fired linings.Supplied as dry oxide or pre-blended by partner plants.
KILN FURNITURESetters & SaggarsG-5073 sub-micronDense Cr₂O₃ wash coats and body additions for kiln furniture that must not react with the ware — electronics and technical ceramics in particular.See the Nano Series for ultrafine options.

Castables and ramming mixes are formulated around particle packing, not colour. Bimodal and trimodal distributions built from the windows above raise green density, tighten fired porosity and lift hot strength — which is why the D50 window, not the shade, is the first specification to lock.

SLAG RESISTANCEMECHANISM

Slag resistance is not a coating property — it is a thermodynamic one. Here is the mechanism, because it is the reason the specification exists.

01

SLOW DISSOLUTION

Cr₂O₃ dissolves into fayalite (2FeO·SiO₂) and FeO-rich melts only slowly. Where periclase goes into solution fast, chrome oxide holds the hot face.

02

SPINEL SKIN

Chromite spinel (Mg,Fe)(Cr,Al)₂O₄ precipitates at the reaction front and thickens the melt boundary layer — the attack self-limits.

03

LOW WETTABILITY

Cr₂O₃-bearing refractories hold a high contact angle against FeO-rich slag: the slag beads rather than wets, so it cannot infiltrate porosity and erode the bond.

The practical result is a dense, self-sealing hot face: early erosion slows to a fraction of its initial rate, and the lining survives campaigns that strip unprotected periclase in weeks. That mechanism is why chrome-magnesia remains the standard in RH degassers, converter tuyere zones and cement burning zones — see the refractory engineering guide and the DELIKEOXIDE series page.

QUALITYCONTROL

Every DELIKEOXIDE lot ships with a CoA: Cr₂O₃ purity, D50 by laser diffraction, Cr(VI) by ISO 4621/ICP, water-soluble salts and sieve residue.

Batch traceability

The batch number on each 25 kg bag resolves to the raw-material record, the kiln log and the QC file — from oxide ore to pallet. ISO 9001 quality system, third-party testing on request. Compare against our pigment grades if your requirement is colour, or contact our engineers at sales@chromeoxidegreen.com.

FREQUENTLY ASKEDQUESTIONS

Both tiers deliver identical particle-size windows and sintered chemistry. The standard tier (G-5001 / G-5002 / G-5003 / G-5006) holds Cr₂O₃ ≥99 % with Cr(VI) ≤200 ppm; the Low-Cr(VI) tier (G-5891 / G-5899 / G-5996 / G-5070 / G-5073) caps hexavalent chromium at ≤5 ppm for plants enforcing strict occupational-exposure or waste-classification limits.
Use the coarse window for the load-bearing skeleton — G-5006 (D50 4–8 μm) or G-5899 (D50 3–8 μm) — and pack the voids with fines such as G-5001 (1.2 μm) or micropowder G-5070 (0.1–3 μm) for maximum green density and hot strength.
Cr₂O₃ dissolves only slowly into fayalite melts, chromite spinel precipitates at the reaction front, and the refractory holds a high contact angle against FeO-rich slag — it beads instead of wetting, so it cannot infiltrate porosity. Field result: RH degasser campaign life extended 30–50 %.
Cr₂O₃ melts at 2435 °C, and our grades serve continuously above 1700 °C in chrome-magnesia systems. The practical ceiling is set by the surrounding bond phase and matrix, not by the chrome oxide itself.
Every 25 kg bag carries a batch number that resolves to a full production record, plus a CoA covering Cr₂O₃ purity, D50 by laser diffraction, Cr(VI) by ISO 4621/ICP, water-soluble salts and sieve residue. Per-grade TDS and REACH-compliant SDS are available on request.

RELATEDREADING